Silly putty in 1940

  • Period: to

    Silly putty

    In 1943, the chemical engineer for General Electric added a bit of boric acid to silicon oil. He noticed that the compound polymerized to form a resilient, flexible material that was almost like rubber. But the substance tended to melt, and it couldn't hold a solid shape